FAQ
  • Q Mirror Coating Operation Process
    Operation (three-coat & three -bake)

    A.  Metal → coating pre-treatment
    (First coat) primer coating →
    (first bake) baking temperature: 160 ° C-180 ° C
    (Second coat) Nanometer Silver Coating(NSC) K1, water, K2, water, AB, water S, water
     → (second bake) baking 100 ° C
    (Third coat) metal topcoat → (third bake) baking 160 ° C-180 ° C

     
    B.  Plastic → removing oil and static
    (First coat) PU primer coating → (first bake) baking temperature: 70 ° C
    (Second coat) Nanometer Silver Coating(NSC) K1, water, K2, water, AB, water S, water
    → (second bake) baking 70 ° C
    (Third coat) PU topcoat → (third bake) baking 70 ° C

     
    C.  Wood → drying and sealer
    (First coat) PU primer coating → (first bake) baking temperature: 50 ° C
    (Second coat) Nanometer Silver Coating(NSC) K1, water, K2, water, AB, water S, water
     → (second bake) baking 50 ° C
    (Third coat) PU topcoat → (third bake) baking 50 ° C